Ross & Catherall manufacturing capabilities

  • Advanced Vacuum Induction Melting (VIM) from 50 to 9,000 kg (110 lb to 20000 lb)Advanced Vacuum Induction Melting (VIM) from 50 to 9,000 kg (110 lb to 20000 lb)
  • Air Melt up to 3000 kg (6,600 lb) Melt CapacityAir Melt up to 3000 kg (6,600 lb) Melt Capacity
  • Alloys for Directionally Solidified (DS) and Single Crystal (SX) ApplicationsAlloys for Directionally Solidified (DS) and Single Crystal (SX) Applications
  • Cobalt, Nickel and Iron Base SuperalloysCobalt, Nickel and Iron Base Superalloys
  • Super Alloys for Powder Additive ManufacturingSuper Alloys for Powder Additive Manufacturing
  • Barstock Diameters from 41 to 175 mm (1 5/8 in to 7 in.)Barstock Diameters from 41 to 175 mm (1 5/8 in to 7 in.)
  • Billet Cut to Weight, Notch, Fractured or Rotary CutBillet Cut to Weight, Notch, Fractured or Rotary Cut
  • Ground and Shot Blast Finish to Customer SpecificationsGround and Shot Blast Finish to Customer Specifications
  • Specialty / R+D Melts up to 40kgSpecialty / R+D Melts up to 40kg

But whether it’s small or large volume production, all nickel, cobalt, and iron base alloys are produced by either vacuum induction or air induction melting to the industry’s most stringent specifications.