Alloy | Description | Specification | EN |
---|---|---|---|
CLA 1A | Carbon Steels | 050A22 | 3 |
CLA 2B | - | 060A32 | 5 |
CLA 1C | - | 060A42 | 8 |
CLA 2 | 1/5% Mn Steel | 150M19 | 14A |
CLA 3 | 700MPa to 850MPa alloy steel | 816M40 | 24 |
CLA 4 | 850MPa to 1.000MPa alloy steel | 823M31 | - |
CLA 5A | Hig Tensile Steels | 823M31 | - |
CLA 5B | - | - | - |
CLA 7 | 3% CR-Mo steel | 722M24 | 29 |
CLA 8 | Case hardening carbon steel | 060A40 | 8 |
CLA 9 | Case hardening carbon steel | 080A15 | 32 |
CLA 10 | 3% Ni case hardening carbon steel | 722M24 | 33 |
CLA 11 | 3% Cr-Mo nitriding steel | 722M24 | 40 |
CLA 12 A&B | 1% Cr abrasion resisting steels | - | - |
CLA 12 C | - | - | - |
CLA 13 | Ni-Mo steel | 655H17 | 34 |
Alloy | C | Fe | Si | Mn | Ni | Co | Cr | Mo | Al | Ti | Others |
---|---|---|---|---|---|---|---|---|---|---|---|
CLA 1A | 0.20 | Bal | 0.40 | 0.70 | <0.4 | - | <0.3 | <0.1 | - | - | - |
CLA 2B | 0.30 | Bal | 0.40 | 0.70 | <0.4 | - | <0.3 | <0.1 | - | - | - |
CLA 1C | 0.40 | Bal | 0.40 | 0.70 | <0.4 | - | <0.3 | <0.1 | - | - | - |
CLA 2 | 0.22 | Bal | 0.35 | 1.45 | <0.4 | - | <0.3 | <0.1 | - | - | - |
CLA 3 | - | Bal | - | - | - | - | - | - | - | - | Composition by agreement with purchaser |
CLA 4 | - | Bal | - | - | - | - | - | - | - | - | Composition by agreement with purchaser |
CLA 5A | - | Bal | - | - | - | - | - | - | - | - | Composition by agreement with purchaser |
CLA 5B | - | Bal | - | - | - | - | - | - | - | - | Composition by agreement with purchaser |
CLA 7 | 0.20 | Bal | 0.55 | 0.45 | <0.4 | - | 3.00 | 0.50 | - | - | - |
CLA 8 | 0.41 | Bal | 0.40 | 0.65 | <0.4 | - | 3.00 | 0.50 | - | - | - |
CLA 9 | 0.14 | Bal | 0.40 | 0.80 | <0.4 | - | <0.3 | <0.1 | - | - | - |
CLA 10 | 0.14 | Bal | 0.40 | 0.45 | 3.10 | - | <0.3 | <0.1 | - | - | - |
CLA 11 | 0.25 | Bal | 0.55 | 0.45 | <0.4 | - | 3.20 | 0.55 | - | - | V <0.02, Sn <0.03 |
CLA 12 A&B | 0.50 | Bal | 0.55 | 0.75 | <0.4 | - | 1.00 | <0.1 | - | - | - |
CLA 12 C | 0.60 | Bal | 0.55 | 0.75 | <0.4 | - | 1.15 | 0.30 | - | - | - |
CLA 13 | 0.16 | Bal | 0.40 | 0.50 | 1.75 | - | <0.3 | 0.25 | - | - | - |
Ross & Catherall Ltd 2013. All rights reserved. No copying is permitted without prior authorisation. Information in this document is subject to change without notice.
Ross & Catherall has made a diligent effort to ensure the specifications listed are accurate as of December 2013. However, the company assumes no liability for errors or omissions, or use or suitability of specifications for particular applications.
Please consult the appropriate issuing organisation to confirm specifications before ordering.
*Typical Chemical composition given for indication only
All typically 0.035max Sulfur/Phosphorus, 0.3max Copper
BS3146 Pt II:1975 | Description | British/USA |
---|---|---|
ANC 1A | 13%Cr martensitic steels | 410C21 |
ANC 1B | - | 420C29 |
ANC 1C | - | - |
ANC 2 | 18% 2%Ni martensitic steels | S80 |
ANC 3A | 18%Cr8%Ni austenitic steels | 317 |
ANC 3B | - | 347 |
ANC 4A | 18%Cr11%Ni3%Mo austenitic steels | 317 |
ANC 4B | - | 316 |
ANC 4C | - | 318 |
ANC 5A | Nickel chromium steels | 310C45 |
ANC 5B | - | 331C60 |
ANC 5C | - | 334C11 |
ANC 6A | Nickel chromium steels | 309C30 |
ANC 6B | - | 309C30 |
ANC 6C | - | - |
ANC 20 | CrNiCuMo PH steels | FV520 |
ANC 21 | CrNiCuMo PH steels | - |
ANC 22 | CrNiCuMo PH steels | 17-4PH |
BS3146 Part II:1975 | C | Fe | Si | Mn | Ni | Co | Cr | Mo | Al | Ti | Others |
---|---|---|---|---|---|---|---|---|---|---|---|
ANC 1A | 0.10 | Bal | 0.70 | 0.70 | <1.0 | - | 12.50 | - | - | - | S&P <0.035 |
ANC 1B | 0.16 | Bal | 0.70 | 0.70 | <1.0 | - | 12.50 | - | - | - | S&P <0.035 |
ANC 1C | 0.25 | Bal | 0.70 | 0.60 | <1.0 | - | 12.50 | - | - | - | S&P <0.035 |
ANC 2 | 0.20 | Bal | 0.60 | 0.60 | 2.00 | - | 17.50 | - | - | - | S&P <0.035 |
ANC 3A | 0.08 | Bal | 1.50 | 1.50 | 10.00 | - | 18.00 | - | - | - | S&P <0.035 |
ANC 3B | 0.08 | Bal | 1.50 | 1.50 | 10.00 | - | 18.00 | - | - | - | Nb=0.90, S&P <0.035 |
ANC 4A | 0.06 | Bal | 1.00 | 1.50 | 12.50 | - | 19.00 | 3.50 | - | - | S&P <0.035 |
ANC 4B | 0.06 | Bal | 1.00 | 1.50 | 11.20 | - | 18.50 | 2.50 | - | - | S&P <0.035 |
ANC 4C | 0.08 | Bal | 1.00 | 1.50 | 11.20 | - | 18.50 | 2.50 | - | - | Nb=0.90, S&P <0.035 |
ANC 5A | 0.30 | Bal | 1.50 | 1.50 | 18.50 | - | 24.00 | - | - | - | - |
ANC 5B | 0.35 | Bal | 2.00 | 1.50 | 38.00 | - | 20.00 | - | - | - | - |
ANC 5C | 0.50 | Bal | 2.00 | 1.50 | 57.00 | - | 13.00 | - | - | - | - |
ANC 6A | 0.20 | Bal | 1.70 | 0.60 | 11.00 | - | 22.50 | - | - | - | S&P <0.035 |
ANC 6B | 0.23 | Bal | 1.50 | 0.60 | 11.00 | - | 22.50 | - | - | - | W=3.00, S&P <0.035 |
ANC 6C | 0.10 | Bal | 1.50 | 0.60 | 14.00 | - | 22.50 | - | - | - | W=3.00, S&P <0.035 |
ANC 20 | 0.04 | Bal | 1.50 | 0.60 | 4.50 | - | 14.00 | 1.00 | - | - | Cu=2.25, Nb <0.5, P&S <0.025 |
ANC 21 | <0.05 | bal | 0.50 | 0.50 | 5.25 | - | 26.00 | 2.00 | - | - | Cu=3.00 N <0.1, P&S <0.050 |
ANC 22 | 0.04 | Bal | 0.70 | 0.40 | 4.00 | - | 16.00 | - | - | - | Cu=3, Nb=0.3, S <0.03, P<0.035 |
Ross & Catherall Ltd 2013. All rights reserved. No copying is permitted without prior authorisation. Information in this document is subject to change without notice.
Ross & Catherall has made a diligent effort to ensure the specifications listed are accurate as of December 2013. However, the company assumes no liability for errors or omissions, or use or suitability of specifications for particular applications.
Please consult the appropriate issuing organisation to confirm specifications before ordering.
*Typical Chemical composition given for indication only
BS3146 Part II:1975 | Description | British/USA |
---|---|---|
ANC 8 | 20%Cr 0.4%%i | N75 |
ANC 9 | 20%Cr 2.5%Ti 1.2%AI | N80 |
ANC 10 | 20%Cr 16.5Co 2.4%Ti 1.3%AI | N90 |
ANC11 | 21%Cr 10%Mo 10%Co | C242 |
ANC 15 | 28%Mo | Hastelloy B |
ANC 16 | 17%Mo 16.5%Cr 4.5%W | Hastelloy C |
ANC 17 | 9%i 3%Cu | Hastelloy D |
ANC 18 | A 31%Cu 1-4%Si | Monel |
ANC 18B | - | Monel H |
ANC 18C | - | Monel H |
ANC 19 | Cr-Nb-Mo-Fe-W | PE10/MC102 |
BS3146 Part II:1975 | C | Fe | Si | Mn | Ni | Co | Cr | Mo | Al | Ti | Others |
---|---|---|---|---|---|---|---|---|---|---|---|
ANC 8 | 0.12 | <5.00 | 0.60 | 0.60 | Bal | - | 20.00 | - | 0.15 | - | - |
ANC 9 | 0.07 | <2.00 | 0.60 | 0.60 | Bal | <2.00 | 20.00 | - | 1.20 | - | - |
ANC 10 | 0.09 | <2.00 | 0.60 | 0.60 | Bal | 16.50 | 19.50 | - | 1.30 | - | - |
ANC 11 | 0.34 | <1.00 | 0.32 | 0.32 | Bal | 10.00 | 20.50 | 10.00 | <0.20 | - | - |
ANC 15 | 0.07 | 5.50 | 0.85 | 0.85 | Bal | - | - | 27.00 | - | - | S<0.030 |
ANC 16 | 0.10 | 6.00 | 0.85 | 0.85 | Bal | - | 16.50 | 16.50 | - | - | W=4.00, S<0.030 |
ANC 17 | 0.08 | <2.00 | 9.25 | 0.85 | Bal | - | - | - | - | - | Cu=3.00, S<0.030 |
ANC 18A | 0.20 | <3.00 | 1.00 | 1.00 | Bal | - | - | - | - | - | Cu=31.00, Mg=0.10, S<0.050 |
ANC 18B | 0.10 | <3.00 | 2.75 | 1.00 | Bal | - | - | - | - | - | Cu=31.00, Mg=0.10, S<0.050 |
ANC 18C | 0.10 | <3.00 | 4.00 | 1.00 | Bal | - | - | - | - | - | W=2.0, Nb+Ta+6.60, S<0.015 |
ANC 19 | 0.04 | 3.00 | 0.30 | 0.30 | Bal | <2.00 | 20.00 | 6.00 | - | - | - |
BS3146 Part II:1975 | Description | British/USA |
---|---|---|
ANC 13 | 26%Cr 10%Ni 7%W | Stellite 31/X40 |
ANC 14 | 27%Cr 5.5%Mo 2.7%Ni | Stellite 8 |
BS3146 Part II:1975 | C | Fe | Si | Mn | Ni | Co | Cr | Mo | Al | Ti | Others |
---|---|---|---|---|---|---|---|---|---|---|---|
ANC 13 | 0.48 | <2.00 | 0.75 | 0.75 | 10.50 | Bal | 25.50 | - | - | - | W = 7.50 |
ANC 14 | 0.25 | <3.00 | 0.70 | 0.70 | 2.75 | Bal | 27.50 | 5.50 | - | - | - |